The KZ tank Full send !

 

KZ tank part 2...... 


Well I got the dent out. Unfortunately the steel was to strong for my dent puller. It broke. So I resorted to welding tabs onto the tank and making a puller. This has moved metal but its tough!


So, in order of severity I tried; Glue and slide hammer


  • Heat and ice ( this worked a little )

  • Air pressure ( this had no effect except to raise the seam and spread the tank Even though I had ratchet straps holding the tank shape .. )

  • Air pressure, heat and Ice … nothing

  • Welding studs to the dent and using a slide hammer ( this moved some metal but broke my slide hammer)

  • welding studs, slide hammer, heat and ice. ( this worked but the metal was too tough so only small movement in the metal )

  • welding studs , a 12mm dia stud puller, air pressure , heat and ice ….( finally I could move things


As of today, I have the basic shape in place, lots of little tiny dings and dents that need to be smoothed off, Ill try stud welding heat and ice , there is a deep dent that will be difficult to move, BUT the positive the tank can be saved . Unfortunately, there are a few pin holes here the weld pulled out and a seam that split. I hope these can be welded .

 いや〜、なんとか凹みは直せました!
ただ、タンクの鉄がめちゃくちゃ強くて、デントプラーがまさかの破損…。
仕方ないので、タンクにタブを溶接して、自作のプーラーを作りました。これで少しずつ金属を動かせましたが、いや〜硬い!

試した順番をざっと書くと、こんな感じです👇

  • 接着式スライドハンマー

  • 加熱+氷(ちょっとだけ効果あり)

  • エア圧(効果ゼロ。むしろ継ぎ目が持ち上がってタンクが広がるという悲劇…💦 ラチェットストラップで形を押さえてたのに!)

  • エア圧+加熱+氷(これも全くダメ)

  • スタッドを溶接してスライドハンマーで引っ張る(少し動いたけど、スライドハンマーが壊れた…)

  • スタッド溶接+スライドハンマー+加熱+氷(少しだけ動いたけど、鉄が硬すぎて進まない)

  • スタッド溶接+直径12mmのスタッドプーラー+エア圧+加熱+氷(ようやく動き始めた!)

今日のところは、タンクの基本形はだいたい戻りました。
あとは小さな凹みやキズを少しずつ整えていく作業です。
スタッド溶接+加熱+氷の組み合わせでもう少し滑らかにできると思います。

深めの凹みがひとつあって、そこはちょっと手ごわそうですが、ポジティブに言えば「このタンク、まだ救える!」って感じです✨

ただ残念なのは、スタッドを引っ張った時に小さなピンホールがいくつかできてしまったのと、継ぎ目が少し裂けたところ。
なんとか溶接で修復できるといいなと思ってます。